Toluene diisocyanate manufacturer Knowledge The most common causes of concrete segregation

The most common causes of concrete segregation

◆A low sand rate or a low content of fine particles in the sand will result in low water retention of concrete. A high mud content in the sand will easily cause slurry settlement, that is, “grabbing the bottom.”

◆The total amount of cementitious materials is small, and the slurry volume is less than 300L/m3;

◆The stone gradation is poor, or the stones are of a single particle size;

◆Large water consumption makes the viscosity of the concrete mixture low;

◆The amount of admixture is too large, or the admixture has low viscosity and poor water retention;

◆Use slag or slag Cement itself has poor water retention and is prone to bleeding and segregation.

</p

This article is from the Internet, does not represent the position of Toluene diisocyanate reproduced please specify the source.https://www.allhdi.com/archives/11442

author:

Previous article
Next article
Contact Us

Contact us

+86 - 152 2121 6908

Online consultation: QQ交谈

E-mail: sales@newtopchem.com

Working hours: Monday to Friday, 9:00-17:30, closed on holidays
Follow wechat
Scan wechat and follow us

Scan wechat and follow us

Back to top
Home
E-mail
Products
Search